Understanding and preventing common welding defects

Welding ABC

Understanding and preventing common welding defects

15 February 2024

Welding demands precision, but even skilled welders can encounter defects. Understanding common welding issues is critical to ensure high-quality results. Here are some frequent welding defects and how to avoid them.

Susanna Norja

Susanna Norja
Author

Susanna Norja

Editor-in-chief of the Kemppi blog, content producer, and Social Media Manager at Kemppi until March 2024.

More blog posts

What Shielding Gas for TIG Welding?

What Shielding Gas for TIG Welding?

How to choose the right shielding gas for TIG welding? Is there a gas suitable for any material that can be TIG welded?

Manual welding

MIG/MAG welding arc types

MIG/MAG welding arc types

In MIG/MAG welding, the mode of material transfer between the filler wire and the weld pool changes in line with the welding current.

Welding ABC

Choosing the right gas nozzle length for MIG (GMAW) welding

Choosing the right gas nozzle length for MIG (GMAW) welding

Gas nozzle length is an important feature in a MIG welding torch because nozzle length has an effect in contact tip heat load, contact tip spatter protection and welding current.

Welding ABC

Eurosatory 2026 Shows That the Future of Defence Is Built in Steel

Eurosatory 2026 Shows That the Future of Defence Is Built in Steel

Eurosatory 2026 highlighted a clear shift in modern defence manufacturing. While defence systems are becoming more digital, networked, and autonomous, their foundation remains physical. From armoured vehicles and artillery to industrial resilience, welding quality, steel structures, and production discipline remain paramount to defence readiness.

Digitalization, Innovation

What Built to Last Really Means in Defence and Marine Welding

What Built to Last Really Means in Defence and Marine Welding

Critical defence and military vessels and marine structures are built for decades of demanding service. This article explores what 'built to last' means in welding, from harsh-condition reliability and repeatable weld quality to traceability across long vessel lifecycles.

Innovation, Digitalization

How Kemppi Supports Defence Shipyard Welding from Steel to Aluminium

How Kemppi Supports Defence Shipyard Welding from Steel to Aluminium

Kemppi X5 FastMig supports reliable MIG/MAG welding, controlled heat input, traceability, and repeatable weld quality across steel, aluminium, and challenging production conditions.

Subscribe to our newsletter and be among the first to know the latest from Kemppi.

Select contact type

By subscribing, you agree to receive marketing emails from Kemppi.

The forerunners of arc welding

Kemppi is the design leader of the arc welding industry. Kemppi is the design leader in the arc welding industry. We are committed to boosting the quality and productivity of welding by continuous development of the welding arc and by working for a greener and more equal world. Kemppi supplies sustainable products, digital solutions, and services for professionals from industrial welding companies to single contractors. The usability and reliability of our products is our guiding principle. We operate with a highly skilled partner network covering over 70 countries to make its expertise locally available. Headquartered in Lahti, Finland, Kemppi employs over 650 professionals in 16 countries and has a revenue of 209 MEUR in 2023.

Kemppi – Designed for welders

Copyright © 2025 Kemppi Oy