How to Avoid the Most Common MIG/MAG Welding Defects

Sveise-ABC

How to Avoid the Most Common MIG/MAG Welding Defects

15. februar 2021

The quality requirements in welding production increase with the optimization of structures as well as the development of materials and welding processes. Welding defects can, at worst, cause serious accidents and structural damage, so it is important to avoid them and understand the mechanisms that create them. In this text, we present the most common MIG/MAG welding defects and the ways to best avoid them.

Reetta Verho

Reetta Verho
Author

Reetta Verho

Manager, Welding Services at Kemppi Oy. International Welding Engineer (IWE) who is an active member in ISO standardization committees. Board member in The Welding Society of Finland. Passionate about welding quality and the development of welding production. Member of: K105 National mirror committee for welding, ISO/TC44/SC10 Quality management in the field of welding ISO/TC44/SC11 Qualification requirements for welding and allied processes personnel.

Flere blogginnlegg

Calculation of heat input in MIG/MAG welding

Calculation of heat input in MIG/MAG welding

The new welding procedure test standard, EN-ISO 15614-1:2017, provides recommendations for the measurement and calculation of heat input. In concrete terms, what does this mean for MIG/MAG welding? And how can workshops carry out these calculations in practice?

Sveise-ABC

Welding value with X5 FastMig

Welding value with X5 FastMig

Small improvements in welding efficiency can positively influence overall productivity and establish valuable cost savings. By investing in robust, reliable, and versatile equipment, you can improve and better manage welding project costs.

Manuell sveising

WeldEye enables remote work in welding production

WeldEye enables remote work in welding production

Managing welding production with a cloud-based software solution has considerable advantages. For one, it gives work supervisors or quality assurance teams the convenience of working remotely from home. It increases transparency, quality and efficiency, thanks to improved information flow and traceability. The welders also receive immediate feedback on their work.

Digitalisering

Kemppi's advanced welding processes: TIG and stick welding (MMA)

Kemppi's advanced welding processes: TIG and stick welding (MMA)

In TIG welding, process development has mainly focused on modifying the current modes in different situations. In practice, this means variations of pulse and AC welding, as well as ignition or tack welding. In the case of pulse welding, the welding machine user has numerous choices, as the adjustment possibilities for these process variations are highly versatile.

Sveise-ABC, Manuell sveising

Magnetism in welding: how to deal with magnetic blow

Magnetism in welding: how to deal with magnetic blow

When welding ferritic steels, especially high-strength grades, magnetic blow can become a real challenge. This phenomenon occurs when magnetic fields interfere with the welding arc, causing instability, spatter, and sometimes making welding almost impossible.

Manuell sveising

Sveiseytelsen starter med sveisepistolen

Sveiseytelsen starter med sveisepistolen

Vi ser nærmere på den mest håndgripelige delen av hver sveis.

Manuell sveising

Abonner på nyhetsbrevet vårt og vær blant de første som får de siste nyhetene fra Kemppi.

Select contact type

Ved å abonnere godtar du å motta markedsførings-e-poster fra Kemppi.

Foregangsbedriften innen lysbuesveising

Kemppi er designleder i sveiseindustrien. Vi er forpliktet til å øke kvaliteten og produktiviteten til sveiseren ved kontinuerlig utvikling av lysbuen og ved å arbeide for en grønnere og mer likeverdig verden. Kemppi leverer bærekraftige produkter, digitale løsninger og tjenester til fagfolk fra industrielle sveisebedrifter til enkeltentreprenører. Brukervennligheten og påliteligheten til produktene våre er vårt ledende prinsipp. Vi opererer med et svært dyktig partnernettverk som dekker over 70 land for å gjøre sin ekspertise lokalt tilgjengelig. Kemppi har hovedkontor i Lahti, Finland, og sysselsetter over 650 fagfolk i 16 land og har en omsetning på 209 MEUR.